Is anyone interested in hydrographed yo-yos?

Not that ugly, if you take the caps out. The caps do not mix.

Also this would look better on aluminium.

Ahhh ok. I had a Camo Hitman once. The stuff’s not very durable - about as tough as paint.

Unless he has a special coat to keep it durable.

Can you do it in the cup while leaving the rest anno’d?

This is how hydrographing works. As such, just doing the inner cup would be very impractical.

Do you have a special clear coat or something to protect it from dings, or protect it at all?

i do! i plane to give it a coat of clear to harden up the surface!

I just read that the Texture on the Yomega Glide Is easily chip able, so I assume it is this.

How would you get it off your hand???

haha, not really sure how that would be taken off

Rick from the MadHouse here:

Just wanted to clarify this again…

Yomega most recently and others similar to it, most notably the Duncans and yoyoJams from a few years back are using Hydro Graphics on their yoyos.
      MadHouse is not and does not.
Hydro is not very durable…

We use a completely different process. Ours is way more durable and long lasting.

Check it!

–Rick

O_o