How do they get those aluminum inserts in the protostar?

Just wondering, as I have no experience with bimetals or plastics with metal rings, but does YYF for instance glue aluminum rings in plastics like the protostar or do they like snap in or what? Just curious. I would think gluing would be less precise re. weight, but maybe it’s nominal….

Thanks!

2 Likes

I have no idea. My guess is compression fitting, basically snapping like you suggested. Again, I’m guessing.

3 Likes

Press fit