# Yoyo Finish Durability

**URL:** <https://forums.yoyoexpert.com/t/yoyo-finish-durability/302671>\
**Category:** General Yo-Yo\
**Created:** [May 23, 2019, 1:59am UTC](https://forums.yoyoexpert.com/t/yoyo-finish-durability/302671 "2019-05-23T01:59:45Z")\
**Posts on this page:** 12\
**Page:** 2

<div class="post-metadata">

**Author:** ![RyoCanCan](https://sea1.discourse-cdn.com/flex015/user_avatar/forums.yoyoexpert.com/ryocancan/32/163437_2.png) [@RyoCanCan](https://forums.yoyoexpert.com/u/RyoCanCan)\
**Post date:** [May 24, 2019, 2:57pm UTC](https://forums.yoyoexpert.com/t/yoyo-finish-durability/302671/21 "2019-05-24T14:57:10Z")

</div>

Yeah, very true.

---

<div class="post-metadata">

**Author:** ![Jhammond93](https://sea1.discourse-cdn.com/flex015/user_avatar/forums.yoyoexpert.com/jhammond93/32/53095_2.png) [@Jhammond93](https://forums.yoyoexpert.com/u/Jhammond93)\
**Post date:** [May 24, 2019, 5:07pm UTC](https://forums.yoyoexpert.com/t/yoyo-finish-durability/302671/22 "2019-05-24T17:07:08Z")

</div>

With What little reading I did, it’s my understanding that if done properly, cerakote can actually come out thinner. @TheThrowingGnome never hurts to ask. In my experience, gun smiths are usually pretty laid back guys. They can also do some really impressive work with cerakote.

---

<div class="post-metadata">

**Author:** ![Jhammond93](https://sea1.discourse-cdn.com/flex015/user_avatar/forums.yoyoexpert.com/jhammond93/32/53095_2.png) [@Jhammond93](https://forums.yoyoexpert.com/u/Jhammond93)\
**Post date:** [May 24, 2019, 5:10pm UTC](https://forums.yoyoexpert.com/t/yoyo-finish-durability/302671/23 "2019-05-24T17:10:53Z")

</div>

As far as vibe goes, I feel as though if you take your time and do it right it shouldn’t be too hard to get a good even coat. The only challenge I can see is finding a way to hang the YoYo in the air while painting, and baking. Might need to sacrifice an axle, or get a bolt from the hardware store to attach a string.

---

<div class="post-metadata">

**Author:** ![TheThrowingGnome](https://sea1.discourse-cdn.com/flex015/user_avatar/forums.yoyoexpert.com/thethrowinggnome/32/14231_2.png) [@TheThrowingGnome](https://forums.yoyoexpert.com/u/TheThrowingGnome)\
**Post date:** [May 24, 2019, 6:21pm UTC](https://forums.yoyoexpert.com/t/yoyo-finish-durability/302671/24 "2019-05-24T18:21:52Z")

</div>

Maybe I should Ceracote my already vibey TiShutter instead of stonewashing! :thinking:

---

<div class="post-metadata">

**Author:** ![Jhammond93](https://sea1.discourse-cdn.com/flex015/user_avatar/forums.yoyoexpert.com/jhammond93/32/53095_2.png) [@Jhammond93](https://forums.yoyoexpert.com/u/Jhammond93)\
**Post date:** [May 24, 2019, 6:29pm UTC](https://forums.yoyoexpert.com/t/yoyo-finish-durability/302671/25 "2019-05-24T18:29:15Z")

</div>

Idk what stonewashing is, but a decent cerakote setup doesn’t seem all that crazy. The biggest thing you’ll need is a spray gun with a hopper. Doesn’t need to be anything expensive or crazy.

---

<div class="post-metadata">

**Author:** ![zslane](https://sea1.discourse-cdn.com/flex015/user_avatar/forums.yoyoexpert.com/zslane/32/19816_2.png) [@zslane](https://forums.yoyoexpert.com/u/zslane)\
**Post date:** [May 24, 2019, 6:52pm UTC](https://forums.yoyoexpert.com/t/yoyo-finish-durability/302671/26 "2019-05-24T18:52:04Z")

</div>

I could have taffeta white yoyos!

---

<div class="post-metadata">

**Author:** ![da5id](https://sea1.discourse-cdn.com/flex015/user_avatar/forums.yoyoexpert.com/da5id/32/48214_2.png) [@da5id](https://forums.yoyoexpert.com/u/da5id)\
**Post date:** [May 24, 2019, 6:55pm UTC](https://forums.yoyoexpert.com/t/yoyo-finish-durability/302671/27 "2019-05-24T18:55:06Z")

</div>

No durability benefit from Pyramatte.

---

<div class="post-metadata">

**Author:** ![RyoCanCan](https://sea1.discourse-cdn.com/flex015/user_avatar/forums.yoyoexpert.com/ryocancan/32/163437_2.png) [@RyoCanCan](https://forums.yoyoexpert.com/u/RyoCanCan)\
**Post date:** [May 24, 2019, 7:09pm UTC](https://forums.yoyoexpert.com/t/yoyo-finish-durability/302671/28 "2019-05-24T19:09:45Z")

</div>

To get an even coat you can get one of those photography turntables or a cheap potter’s wheel to spin it while spraying.

---

<div class="post-metadata">

**Author:** ![codinghorror](https://sea1.discourse-cdn.com/flex015/user_avatar/forums.yoyoexpert.com/codinghorror/32/8052_2.png) [@codinghorror](https://forums.yoyoexpert.com/u/codinghorror)\
**Post date:** [May 24, 2019, 7:16pm UTC](https://forums.yoyoexpert.com/t/yoyo-finish-durability/302671/29 "2019-05-24T19:16:27Z")

</div>

> [@Jhammond93](#):
>
> Idk what stonewashing is

This is one case where the description is kinda accurate. Throw it in a tumbling mechanism (a “washer”) with a bunch of stones and let it tumble for a while.

---

<div class="post-metadata">

**Author:** ![Jhammond93](https://sea1.discourse-cdn.com/flex015/user_avatar/forums.yoyoexpert.com/jhammond93/32/53095_2.png) [@Jhammond93](https://forums.yoyoexpert.com/u/Jhammond93)\
**Post date:** [May 24, 2019, 8:02pm UTC](https://forums.yoyoexpert.com/t/yoyo-finish-durability/302671/30 "2019-05-24T20:02:08Z")

</div>

Nice! What’s the benefit of that?

---

<div class="post-metadata">

**Author:** ![codinghorror](https://sea1.discourse-cdn.com/flex015/user_avatar/forums.yoyoexpert.com/codinghorror/32/8052_2.png) [@codinghorror](https://forums.yoyoexpert.com/u/codinghorror)\
**Post date:** [May 24, 2019, 8:11pm UTC](https://forums.yoyoexpert.com/t/yoyo-finish-durability/302671/31 "2019-05-24T20:11:15Z")

</div>

There’s a whole topic here about it that got bumped very recently if you look at the latest topics!

---

<div class="post-metadata">

**Author:** ![jasonwongzero](https://sea1.discourse-cdn.com/flex015/user_avatar/forums.yoyoexpert.com/jasonwongzero/32/725_2.png) [@jasonwongzero](https://forums.yoyoexpert.com/u/jasonwongzero)\
**Post date:** [May 24, 2019, 8:24pm UTC](https://forums.yoyoexpert.com/t/yoyo-finish-durability/302671/32 "2019-05-24T20:24:50Z")

</div>

In my experience, coating any yoyo with anything other than standard ano or something that is thin liquid applied like a Teflon spray can induce vibe.

I had a ton of yoyos PVD coated by a commercial outfit that does zippo lighters thinking it wouldn’t be an issue and probably 40 percent of my yoyos came back with varying degrees of vibe. It sucked.