# Give your yo-yo a blast finish using your dryer

**URL:** <https://forums.yoyoexpert.com/t/give-your-yo-yo-a-blast-finish-using-your-dryer/298626>\
**Category:** Yo-Yo Mods and Maintenance\
**Created:** [February 8, 2019, 7:46am UTC](https://forums.yoyoexpert.com/t/give-your-yo-yo-a-blast-finish-using-your-dryer/298626 "2019-02-08T07:46:54Z")\
**Posts on this page:** 20\
**Page:** 3

<div class="post-metadata">

**Author:** ![Skwan](https://avatars.discourse-cdn.com/v4/letter/s/dfb087/32.png) [@Skwan](https://forums.yoyoexpert.com/u/Skwan)\
**Post date:** [May 24, 2019, 12:28pm UTC](https://forums.yoyoexpert.com/t/give-your-yo-yo-a-blast-finish-using-your-dryer/298626/42 "2019-05-24T12:28:17Z")

</div>

The coloring from torching is created by formation of an oxide layer on the surface. As its thickness changes, it affects how much it absorbs light of different frequencies. So yes the coloration effect from torching is from a microscopic thin layer on the surface only.

---

<div class="post-metadata">

**Author:** ![adamantiumpops](https://sea1.discourse-cdn.com/flex015/user_avatar/forums.yoyoexpert.com/adamantiumpops/32/198285_2.png) [@adamantiumpops](https://forums.yoyoexpert.com/u/adamantiumpops)\
**Post date:** [May 24, 2019, 5:15pm UTC](https://forums.yoyoexpert.com/t/give-your-yo-yo-a-blast-finish-using-your-dryer/298626/43 "2019-05-24T17:15:24Z")

</div>

Ok fam I’m gonna do it tonight or tomorrow to my VERY torched TiHawk. Only question I have before I start is, will MousePads fit in my TiHawk? G2 doesn’t have it in their list of throws on the site so I can’t actually look up the response size. I would assume it’s standard 19mm and the MousePads I have will work just fine, but we all know what assuming did to the curious bed-jumping monkey cat.

---

<div class="post-metadata">

**Author:** ![smileypants707](https://sea1.discourse-cdn.com/flex015/user_avatar/forums.yoyoexpert.com/smileypants707/32/19045_2.png) [@smileypants707](https://forums.yoyoexpert.com/u/smileypants707)\
**Post date:** [May 24, 2019, 6:21pm UTC](https://forums.yoyoexpert.com/t/give-your-yo-yo-a-blast-finish-using-your-dryer/298626/44 "2019-05-24T18:21:59Z")

</div>

This is a really cool experiment, thanks for documenting all of this! A few thoughts:

> [@codinghorror](#):
>
> and wrap it in a couple towels

First thing that came to my mind, is to wrap it in a couple of large tube socks. Like, drop the container down into the bottom of the sock, twist the excess top portion a little bit and then fold it back down over the outside. With like two or three socks- one a time.

> [@codinghorror](#):
>
> You will end up with a “worn denim jeans” kinda burnished look if that’s what you are shooting for. Less shiny, more textured.

So basically, similar to pyramatte?

---

<div class="post-metadata">

**Author:** ![smileypants707](https://sea1.discourse-cdn.com/flex015/user_avatar/forums.yoyoexpert.com/smileypants707/32/19045_2.png) [@smileypants707](https://forums.yoyoexpert.com/u/smileypants707)\
**Post date:** [May 24, 2019, 6:42pm UTC](https://forums.yoyoexpert.com/t/give-your-yo-yo-a-blast-finish-using-your-dryer/298626/45 "2019-05-24T18:42:19Z")

</div>

I’m pretty sure they are OD 19mm slim pads

---

<div class="post-metadata">

**Author:** ![codinghorror](https://sea1.discourse-cdn.com/flex015/user_avatar/forums.yoyoexpert.com/codinghorror/32/8052_2.png) [@codinghorror](https://forums.yoyoexpert.com/u/codinghorror)\
**Post date:** [May 24, 2019, 8:04pm UTC](https://forums.yoyoexpert.com/t/give-your-yo-yo-a-blast-finish-using-your-dryer/298626/46 "2019-05-24T20:04:52Z")

</div>

I took some outdoor pics in sun and shade to get a better sense of the resulting “stonewashed” finish, which can be subtle and hard to see in nighttime pics.

 ![IMG_8124](https://us1.discourse-cdn.com/flex015/uploads/yoyoexpert1/original/4X/6/f/6/6f66ca72c052e659a256d8ed399b6fb3e6d5f755.jpeg)

 ![IMG_8123](https://us1.discourse-cdn.com/flex015/uploads/yoyoexpert1/original/4X/8/8/3/88349eaa37cfc5e93b550b9f2e2b0ebf827291eb.jpeg)

---

<div class="post-metadata">

**Author:** ![smileypants707](https://sea1.discourse-cdn.com/flex015/user_avatar/forums.yoyoexpert.com/smileypants707/32/19045_2.png) [@smileypants707](https://forums.yoyoexpert.com/u/smileypants707)\
**Post date:** [May 24, 2019, 8:22pm UTC](https://forums.yoyoexpert.com/t/give-your-yo-yo-a-blast-finish-using-your-dryer/298626/47 "2019-05-24T20:22:02Z")

</div>

Would you recommend this with a black one? And also, is the titanium sealed in any kind of way that is effectively ruined by doing this? You mentioned that the grey and black ones were actually anodized, correct?

---

<div class="post-metadata">

**Author:** ![codinghorror](https://sea1.discourse-cdn.com/flex015/user_avatar/forums.yoyoexpert.com/codinghorror/32/8052_2.png) [@codinghorror](https://forums.yoyoexpert.com/u/codinghorror)\
**Post date:** [May 24, 2019, 8:53pm UTC](https://forums.yoyoexpert.com/t/give-your-yo-yo-a-blast-finish-using-your-dryer/298626/48 "2019-05-24T20:53:27Z")

</div>

> [@smileypants707](#):
>
> Would you recommend this with a black one?

No definitely not

> [@smileypants707](#):
>
> is the titanium sealed in any kind of way that is effectively ruined by doing this?

Titanium is so durable that I don’t think sealing of any kind is really required.

> [@smileypants707](#):
>
> the grey and black ones were actually anodized

Yes the emails I have say “anodized”

---

<div class="post-metadata">

**Author:** ![smileypants707](https://sea1.discourse-cdn.com/flex015/user_avatar/forums.yoyoexpert.com/smileypants707/32/19045_2.png) [@smileypants707](https://forums.yoyoexpert.com/u/smileypants707)\
**Post date:** [May 24, 2019, 9:05pm UTC](https://forums.yoyoexpert.com/t/give-your-yo-yo-a-blast-finish-using-your-dryer/298626/49 "2019-05-24T21:05:01Z")

</div>

> [@codinghorror](#):
>
> Yes the emails I have say “anodized”

> [@codinghorror](#):
>
> Titanium is so durable that I don’t think sealing of any kind is really required.

Doesn’t ano require a chemical seal though? @jasonwongzero do you have any input on this?

---

<div class="post-metadata">

**Author:** ![codinghorror](https://sea1.discourse-cdn.com/flex015/user_avatar/forums.yoyoexpert.com/codinghorror/32/8052_2.png) [@codinghorror](https://forums.yoyoexpert.com/u/codinghorror)\
**Post date:** [May 24, 2019, 9:12pm UTC](https://forums.yoyoexpert.com/t/give-your-yo-yo-a-blast-finish-using-your-dryer/298626/50 "2019-05-24T21:12:46Z")

</div>

You can look up the rationale for the AMS type industrial coatings on titanium if you are curious. It’s really quite optional because Titanium is _crazily_ durable.

---

<div class="post-metadata">

**Author:** ![jasonwongzero](https://sea1.discourse-cdn.com/flex015/user_avatar/forums.yoyoexpert.com/jasonwongzero/32/725_2.png) [@jasonwongzero](https://forums.yoyoexpert.com/u/jasonwongzero)\
**Post date:** [May 24, 2019, 9:28pm UTC](https://forums.yoyoexpert.com/t/give-your-yo-yo-a-blast-finish-using-your-dryer/298626/51 "2019-05-24T21:28:29Z")

</div>

+1 to Coding Horror

Seals and treatments on top of titanium are very much optional and are more for the aesthetics and texture effect as opposed to protection. Ti is supremely durable, especially for abrasion resistance which is what we want for yoyos.

---

<div class="post-metadata">

**Author:** ![codinghorror](https://sea1.discourse-cdn.com/flex015/user_avatar/forums.yoyoexpert.com/codinghorror/32/8052_2.png) [@codinghorror](https://forums.yoyoexpert.com/u/codinghorror)\
**Post date:** [May 24, 2019, 9:34pm UTC](https://forums.yoyoexpert.com/t/give-your-yo-yo-a-blast-finish-using-your-dryer/298626/52 "2019-05-24T21:34:44Z")

</div>

There’s a really good [writeup on this](https://www.finishing.com/library/titanium.html) here

> Titanium alloys in and of themselves have outstanding corrosion resistance so the question is often asked why would anyone have to coat titanium? As a diverse metal finishing house offering nearly 100 different coatings and finishes on all sorts of metal and non-metallic components, Anoplate can emphatically state that corrosion resistance is only one reason for coating parts:
> 
> - We coat parts to improve their appearance including making them shiny or changing their color to give them greater appeal. Parts that go into optical assemblies often get a dull black finish to make them less reflective. Black coatings are also used to impart particular thermal characteristics.
> 
> - Specific coatings such as silver and gold are used to increase surface conductivity while others are used to render a surface non-conductive or more electrically resistant.
> 
> - Anoplate also coats many parts with tin-lead or nickel or silver to assist in joining parts using solder or brazing techniques.
> 
> Often the coating we’re asked to apply is more related to the desired surface characteristics of the assembled component rather than the individual piece, thus surface engineering is probably a more appropriate description of what Anoplate provides.

---

<div class="post-metadata">

**Author:** ![smileypants707](https://sea1.discourse-cdn.com/flex015/user_avatar/forums.yoyoexpert.com/smileypants707/32/19045_2.png) [@smileypants707](https://forums.yoyoexpert.com/u/smileypants707)\
**Post date:** [May 24, 2019, 9:37pm UTC](https://forums.yoyoexpert.com/t/give-your-yo-yo-a-blast-finish-using-your-dryer/298626/53 "2019-05-24T21:37:09Z")

</div>

So is the ano process for titanium different from aluminum? This whole process is still kiiiind of confusing to me, so sorry if these are silly questions.

> [@codinghorror](#):
>
> There’s a really good [writeup on this](https://www.finishing.com/library/titanium.html) here

I literally _just_ read that exact article lol.

---

<div class="post-metadata">

**Author:** ![adamantiumpops](https://sea1.discourse-cdn.com/flex015/user_avatar/forums.yoyoexpert.com/adamantiumpops/32/198285_2.png) [@adamantiumpops](https://forums.yoyoexpert.com/u/adamantiumpops)\
**Post date:** [May 24, 2019, 9:46pm UTC](https://forums.yoyoexpert.com/t/give-your-yo-yo-a-blast-finish-using-your-dryer/298626/54 "2019-05-24T21:46:05Z")

</div>

So… I COULD use mouse pads? Or nah? I also have a couple sets of c3 pads. Unlabeled.

---

<div class="post-metadata">

**Author:** ![smileypants707](https://sea1.discourse-cdn.com/flex015/user_avatar/forums.yoyoexpert.com/smileypants707/32/19045_2.png) [@smileypants707](https://forums.yoyoexpert.com/u/smileypants707)\
**Post date:** [May 24, 2019, 9:48pm UTC](https://forums.yoyoexpert.com/t/give-your-yo-yo-a-blast-finish-using-your-dryer/298626/55 "2019-05-24T21:48:54Z")

</div>

> [@The Ti-Vayder Experience](https://forums.yoyoexpert.com/t/the-ti-vayder-experience/299824/396):
>
> Generic CT bearing (though apparently “licensed”, I dunno how that all works) and regular 19mm slim silicone sticker pads.

I know nothing about “mouse pads”, but if they are the same as [OD?] 19mm slim pads, then yes.

---

<div class="post-metadata">

**Author:** ![adamantiumpops](https://sea1.discourse-cdn.com/flex015/user_avatar/forums.yoyoexpert.com/adamantiumpops/32/198285_2.png) [@adamantiumpops](https://forums.yoyoexpert.com/u/adamantiumpops)\
**Post date:** [May 24, 2019, 9:58pm UTC](https://forums.yoyoexpert.com/t/give-your-yo-yo-a-blast-finish-using-your-dryer/298626/56 "2019-05-24T21:58:24Z")

</div>

Wait that’s for the vayder. I’m talking about the ti hawk

---

<div class="post-metadata">

**Author:** ![codinghorror](https://sea1.discourse-cdn.com/flex015/user_avatar/forums.yoyoexpert.com/codinghorror/32/8052_2.png) [@codinghorror](https://forums.yoyoexpert.com/u/codinghorror)\
**Post date:** [May 24, 2019, 10:01pm UTC](https://forums.yoyoexpert.com/t/give-your-yo-yo-a-blast-finish-using-your-dryer/298626/57 "2019-05-24T22:01:44Z")

</div>

I’m not sure, the newer G2 use standard silicone 19mm sticker sizes, older ones require flowable or some other non-standard thing. Hawk is an older yo-yo so I would _guess_ flowable?

Actually I just looked at my Ti Hawk and it is indeed using a sticker, 100% confirmed, so maybe Jake redesigned that bit for the Ti run?

---

<div class="post-metadata">

**Author:** ![smileypants707](https://sea1.discourse-cdn.com/flex015/user_avatar/forums.yoyoexpert.com/smileypants707/32/19045_2.png) [@smileypants707](https://forums.yoyoexpert.com/u/smileypants707)\
**Post date:** [May 24, 2019, 10:02pm UTC](https://forums.yoyoexpert.com/t/give-your-yo-yo-a-blast-finish-using-your-dryer/298626/58 "2019-05-24T22:02:08Z")

</div>

Oooooooh, my bad. Yeah, I have no idea. Sorry lol

---

<div class="post-metadata">

**Author:** ![adamantiumpops](https://sea1.discourse-cdn.com/flex015/user_avatar/forums.yoyoexpert.com/adamantiumpops/32/198285_2.png) [@adamantiumpops](https://forums.yoyoexpert.com/u/adamantiumpops)\
**Post date:** [May 24, 2019, 10:05pm UTC](https://forums.yoyoexpert.com/t/give-your-yo-yo-a-blast-finish-using-your-dryer/298626/59 "2019-05-24T22:05:15Z")

</div>

> [@codinghorror](#):
>
> sticker, 100% confirmed

Thanks broseph

---

<div class="post-metadata">

**Author:** ![adamantiumpops](https://sea1.discourse-cdn.com/flex015/user_avatar/forums.yoyoexpert.com/adamantiumpops/32/198285_2.png) [@adamantiumpops](https://forums.yoyoexpert.com/u/adamantiumpops)\
**Post date:** [May 24, 2019, 10:51pm UTC](https://forums.yoyoexpert.com/t/give-your-yo-yo-a-blast-finish-using-your-dryer/298626/60 "2019-05-24T22:51:56Z")

</div>

Ok I started it. Dryer too a dump though because it’s overheating, lol. Shaking it manually for a while  
My toddler is helping.

---

<div class="post-metadata">

**Author:** ![MarkD](https://sea1.discourse-cdn.com/flex015/user_avatar/forums.yoyoexpert.com/markd/32/40845_2.png) [@MarkD](https://forums.yoyoexpert.com/u/MarkD)\
**Post date:** [May 24, 2019, 11:05pm UTC](https://forums.yoyoexpert.com/t/give-your-yo-yo-a-blast-finish-using-your-dryer/298626/61 "2019-05-24T23:05:24Z")

</div>

> [@adamantiumpops](#):
>
> My toddler is helping.

yes… YES!!!

[Previous page](https://forums.yoyoexpert.com/t/give-your-yo-yo-a-blast-finish-using-your-dryer/298626.md?page=2)

[Next page](https://forums.yoyoexpert.com/t/give-your-yo-yo-a-blast-finish-using-your-dryer/298626.md?page=4)