# Do different aluminum grades offer different ano’s?

**URL:** <https://forums.yoyoexpert.com/t/do-different-aluminum-grades-offer-different-ano-s/302553>\
**Category:** General Yo-Yo\
**Created:** [May 20, 2019, 10:50pm UTC](https://forums.yoyoexpert.com/t/do-different-aluminum-grades-offer-different-ano-s/302553 "2019-05-20T22:50:59Z")\
**Posts on this page:** 8\
**Page:** 1

<div class="post-metadata">

**Author:** ![Marm](https://sea1.discourse-cdn.com/flex015/user_avatar/forums.yoyoexpert.com/marm/32/46204_2.png) [@Marm](https://forums.yoyoexpert.com/u/Marm)\
**Post date:** [May 20, 2019, 10:50pm UTC](https://forums.yoyoexpert.com/t/do-different-aluminum-grades-offer-different-ano-s/302553/1 "2019-05-20T22:50:59Z")

</div>

As the title says. What I mean by this is, does 6061 ano differently then 7086 and everything in between? Such as 7075. I know for Titanium you can get different finishes not possible on aluminum. I ask because I saw the Cadence ES and to me the fade looks different from other yo-yos and I know the yo-yo is 7068, which is a high grade.

 ![image](https://us1.discourse-cdn.com/flex015/uploads/yoyoexpert1/original/4X/d/d/7/dd7dfab321aca23c97caf1a554889a18e5d5da36.jpeg) [https://ozhiriz.com/gallery/images/sf-yoyos/cadence-6.jpg](https://ozhiriz.com/gallery/images/sf-yoyos/cadence-6.jpg) also: @sfyoyos love the fade 👌

Edit: I don’t know why there is a link, but it just leads to a full screen pic and not a store. Don’t know if this still counts as a violation

---

<div class="post-metadata">

**Author:** ![codinghorror](https://sea1.discourse-cdn.com/flex015/user_avatar/forums.yoyoexpert.com/codinghorror/32/8052_2.png) [@codinghorror](https://forums.yoyoexpert.com/u/codinghorror)\
**Post date:** [May 20, 2019, 10:52pm UTC](https://forums.yoyoexpert.com/t/do-different-aluminum-grades-offer-different-ano-s/302553/2 "2019-05-20T22:52:12Z")

</div>

The “harder” and “denser” Al alloys (7068 / 7075) are more difficult to anodize, yes, I’ve heard this many times.

---

<div class="post-metadata">

**Author:** ![Marm](https://sea1.discourse-cdn.com/flex015/user_avatar/forums.yoyoexpert.com/marm/32/46204_2.png) [@Marm](https://forums.yoyoexpert.com/u/Marm)\
**Post date:** [May 20, 2019, 10:53pm UTC](https://forums.yoyoexpert.com/t/do-different-aluminum-grades-offer-different-ano-s/302553/3 "2019-05-20T22:53:07Z")

</div>

Is this same finish possible on 6061?

---

<div class="post-metadata">

**Author:** ![AndreBoulay](https://sea1.discourse-cdn.com/flex015/user_avatar/forums.yoyoexpert.com/andreboulay/32/69662_2.png) [@AndreBoulay](https://forums.yoyoexpert.com/u/AndreBoulay)\
**Post date:** [May 20, 2019, 10:54pm UTC](https://forums.yoyoexpert.com/t/do-different-aluminum-grades-offer-different-ano-s/302553/4 "2019-05-20T22:54:43Z")

</div>

Yeah to over generalize - typically the higher quality the aluminum is the more difficult it is to anodize.

With that said - it definitely depends on the type of anodizing and the anodizers familiarity with the specific aluminum. But I remember specifically with YoYoJam back on the day the higher quality the aluminum was gave some weird ano issues (including it coming off much easier with thumb grinds since that was always the test for me - hahahaha).

---

<div class="post-metadata">

**Author:** ![Marm](https://sea1.discourse-cdn.com/flex015/user_avatar/forums.yoyoexpert.com/marm/32/46204_2.png) [@Marm](https://forums.yoyoexpert.com/u/Marm)\
**Post date:** [May 20, 2019, 10:56pm UTC](https://forums.yoyoexpert.com/t/do-different-aluminum-grades-offer-different-ano-s/302553/5 "2019-05-20T22:56:08Z")

</div>

The thumb grind problem you mentioned is muy interesante (very interesting)

---

<div class="post-metadata">

**Author:** ![yoyospirit](https://sea1.discourse-cdn.com/flex015/user_avatar/forums.yoyoexpert.com/yoyospirit/32/219875_2.png) [@yoyospirit](https://forums.yoyoexpert.com/u/yoyospirit)\
**Post date:** [May 20, 2019, 11:30pm UTC](https://forums.yoyoexpert.com/t/do-different-aluminum-grades-offer-different-ano-s/302553/6 "2019-05-20T23:30:40Z")

</div>

Didn’t yoyojam use a weird grade aluminum? 2000 grade or something?

---

<div class="post-metadata">

**Author:** ![AndreBoulay](https://sea1.discourse-cdn.com/flex015/user_avatar/forums.yoyoexpert.com/andreboulay/32/69662_2.png) [@AndreBoulay](https://forums.yoyoexpert.com/u/AndreBoulay)\
**Post date:** [May 21, 2019, 2:09am UTC](https://forums.yoyoexpert.com/t/do-different-aluminum-grades-offer-different-ano-s/302553/7 "2019-05-21T02:09:47Z")

</div>

I believe that is accurate. :+1:

---

<div class="post-metadata">

**Author:** ![AngryGumball](https://sea1.discourse-cdn.com/flex015/user_avatar/forums.yoyoexpert.com/angrygumball/32/683872_2.png) [@AngryGumball](https://forums.yoyoexpert.com/u/AngryGumball)\
**Post date:** [May 22, 2019, 4:48am UTC](https://forums.yoyoexpert.com/t/do-different-aluminum-grades-offer-different-ano-s/302553/8 "2019-05-22T04:48:58Z")

</div>

So that explains my string turning blue around the bearing seat/worn ano on the thumb grind lip on my Eneme, or “pocket worn” ano on my Karma 🙂 Karma doesn’t have any dings but it definitely looks well loved as it’s been with me on many occasions!