**Author:** ![jasonwongzero](https://sea1.discourse-cdn.com/flex015/user_avatar/forums.yoyoexpert.com/jasonwongzero/32/725_2.png) [@jasonwongzero](https://forums.yoyoexpert.com/u/jasonwongzero)\
**Post date:** [June 13, 2019, 3:10am UTC](https://forums.yoyoexpert.com/t/anodizing-questions-answered-by-jasonwongzero-loaded-yoyos/301404/60 "2019-06-13T03:10:53Z")

</div>

> [@Blaidd\_Drwg](#):
>
> I know you do not take on projects anymore, but do you have a network of other Anodizer’s who you feel comfortable giving a referral?

Thank you!

> [@The Ti-Vayder Experience](https://forums.yoyoexpert.com/t/the-ti-vayder-experience/299824/803):
>
> When anodizing titanium, is there a risk of altering the balance - i.e. creating vibe? What about etching? My impression would be no, since the oxide layer is very thin but I would love to hear from your experience.

In my experience anodizing titanium creates too thin an oxide layer to create vibe. Same is probably true of etching as well unless you’re doing something really crazy deep… at which point it might be considered milling as opposed to etching, lol.

---